Where crack repairs are required, the cause, extent and width of the cracks should be established in order to provide information for the selection of appropriate materials and methods.
Fine map-cracking which is not structural, and usually shows when wet may be treated with MM Sealer Siloxane to improve aesthetics and prevent water ingress. Cracks in horizontal slabs may be repaired with LVE Repair (low viscosity or gel epoxy) or SFCF Grout (SuperFineCrackFiller) as dictated by the width of the crack. SFCF Grout is a cementitious polymer modified pumpable and injectable slurry with unique crack filling capability. It is suitable for filling cracks greater the 2mm.
For technical data sheets and installation processes request Samson method statements for site instruction.

| Solution | Product Info |
| LVE Repair or Graviject T | Pack size: 1L kit Yield: Dependent on site requirements |

| SFCF Grout | Pack size: 20kg Yield: 1L per 3kg = 2L slurry Water: 30-35% by mass = 6-7L / 20kg Applied by Caulking gun |